文章摘要
宋雨珂,汪小凯,华林.轴类零件内部缺陷超声检测与重构方法研究[J].,2016,35(2):109-115
轴类零件内部缺陷超声检测与重构方法研究
Research on ultrasonic test and reconstruction method of the internal defects in shaft parts
投稿时间:2015-07-13  修订日期:2016-02-26
中文摘要:
      为了探究轴类零件内部缺陷的无损检测方法,本文以曲轴为研究对象,基于超声ALOK技术对其内部多个?2 mm小孔进行了无损检测实验,并建立了相应的声学仿真有限元模型,提出利用声程—角度散点图中的趋势线,可快速判别内部缺陷特征和位置的方法。并且改进了ALOK算法,即采用邻近探头构建的方程或曲线重构缺陷,模拟和实验结果表明使用改进的算法提高了缺陷位置和尺寸的检测精度,通过实验数据重构所得的缺陷位置误差和半径误差分别在2 mm和0.5 mm左右。研究结论对于轴类零件内部缺陷精确定量化无损检测提供了理论和技术指导。
英文摘要:
      A case study has been made on a crankshaft to non-destructively detect its internal defects. Several artificial holes of ?2 mm have been fabricated in the crankshaft and the test has been conducted based on the ultrasonic ALOK technology, and the acoustics simulation has been completed. A method that can quickly judge the feature and the position of internal defects is proposed based on the trend lines in the sound distance-angle scatter diagram. In addition, the ALOK algorithm is amended through adopting the equations or curves established by adjacent probes to reconstruct the defects. The results of simulations and experiments show that the amended algorithm can improve the detection precision of positions and dimensions. The errors of the position and radius of defects reconstructed through experimental data are about 2 mm and 0.5 mm, respectively. The research provides the theory and technical guidance for the quantitative and non-destructive test of internal defects in shaft parts.
DOI:10.11684/j.issn.1000-310X.2016.02.003
中文关键词: 超声ALOK  轴类零件  内部缺陷  声学仿真  重构
英文关键词: Ultrasonic ALOK  Shaft parts  Internal defects  Acoustics simulation  Reconstruct
基金项目:国家863项目(2013AA040201),教育部创新团队(IRT13087)和湖北省科技支撑计划项目(编号:2015BCE083)
作者单位E-mail
宋雨珂* 现代汽车零部件技术湖北省重点实验室(武汉理工大学)汽车零部件技术湖北省协同创新中心 songyuke@whut.edu.cn 
汪小凯 现代汽车零部件技术湖北省重点实验室(武汉理工大学)西安交通大学机械工程学院 wxk0919@163.com 
华林 现代汽车零部件技术湖北省重点实验室(武汉理工大学)汽车零部件技术湖北省协同创新中心 hualin@whut.edu.cn 
摘要点击次数: 2121
全文下载次数: 2490
查看全文   查看/发表评论  下载PDF阅读器